CompositePlyLab / SI
First-ply failure criteria
Compare Max Stress, Max Strain, Tsai–Hill and Tsai–Wu for one ply under an in-plane stress state.
- Reserve factor
- 1.1296
- Tsai–Wu FI
- 0.82521
- Axial σ₁
- 125.59 MPa
- Transverse σ₂
- 24.412 MPa
Pass · Tsai–Wu · Combined
Inputs
| Fiber angle θ | 30 ° |
|---|---|
| Normal stress σx | 145 MPa |
| Normal stress σy | 5 MPa |
| Shear stress τxy | 18 MPa |
| Fiber tension Xt | 1,680 MPa |
| Fiber compression Xc | 1,230 MPa |
| Matrix tension Yt | 48 MPa |
| Matrix compression Yc | 205 MPa |
| In-plane shear S₁₂ | 80 MPa |
| Tsai–Wu interaction F₁₂* | −0.5 |
| Axial modulus E₁ | 142 GPa |
| Transverse modulus E₂ | 10.3 GPa |
| Shear modulus G₁₂ | 7.2 GPa |
| Major Poisson ratio ν₁₂ | 0.27 |
Results
Failure criteria
| Criterion | Index | Reserve | Mode |
|---|---|---|---|
| Max Stress | 0.645272 | 1.54973 | In-plane shear |
| Max Strain | 0.645272 | 1.54973 | In-plane shear |
| Tsai–Hill | 0.679526 | 1.2131 | Combined |
| Tsai–Wu | 0.825214 | 1.12963 | Combined |
Local stress and strain
- Shear τ₁₂
- −51.6218 MPa
- Axial ε₁
- 838.009 µε
- Transverse ε₂
- 2,131.26 µε
- Shear γ₁₂
- −7,169.69 µε