Worked example

Carbon infusion tooling shell

Estimate mixed resin and cured thickness for an eight-ply tooling shell.

Set waste to zero to isolate net matrix mass. Waste changes batch size while the cured section stays fixed.

View live results

Inputs

Layup
g/m²
m²
%
g/cm³
Resin system
g/cm³
%

Live results

SI
Cured stack
1.6162 mm
Mixed batch
1,213.8 g
Resin mass
933.68 g
Hardener mass
280.11 g
Cured stack and batch mass
Cured layup thickness and dry fiber, resin and hardener mass budget 8 plies1.62 mmFiber1,920Resin934Hardener280g
  • Dry fiber
  • Resin
  • Hardener
Fiber weight share of cured part65.868%
0%100% of cured mass

Layup and batch balance

Dry fiber mass
1,920 g
In-part matrix mass
994.909 g
Additional mix for waste
218.88 g
Cured ply thickness
0.20202 mm
Cured areal weight
2,429.09 g/m²
Fiber volume fraction
55 %
Fiber weight fraction
65.8683 %

Model and assumptions

Mf = FAW·A·N · tply = FAW/(1000ρfVf) in mm · Mbatch = Mmatrix(1 + waste).

Use dry fiber areal weight for a single ply and the actual developed part area. The target fiber fraction is a cured-part value. Mixed matrix mass uses the combined resin-system density.

Waste is an additional percentage of the mixed matrix mass needed in the part. The batch split uses weight parts and applies the same ratio to resin retained in the part and waste.

Cured ply thickness follows fiber volume conservation. Press pressure, resin bleed, cure shrinkage and voids affect practical thickness.

Scope. Uniform ply coverage, no void volume and mass-based resin manufacturer ratios. Add process waste from your own feedline, peel ply or bleeder records.

See calculation methods and references