Worked example

A clay test bar through two firing stages

Enter two shrinkage rates from a test bar to see how large the next piece will be after firing.

Edit example inputs

View results
Piece size
cm
cm
cm
Clay and firing schedule
%
%

Wet, bisque and fired dimensions

Total linear shrinkage 10.33%
Wet, bisque and fired profile Total linear shrinkage · 10.33% Front profileWidth at each stageWet · 4.8 cmBisque · 4.49 cmFired · 4.3 cmLength · 12.5 cm → 11.21 cm27.9% volume loss
Wet, bisque and fired profile · Schematic
Wet length
12.5 cm4.92 in
Wet width
4.8 cm1.89 in
Wet height
2 cm0.7874 in
Bisque length
11.7 cm4.61 in
Bisque width
4.49 cm1.77 in
Bisque height
1.87 cm0.737 in
Fired length
11.21 cm4.41 in
Fired width
4.3 cm1.69 in
Fired height
1.79 cm0.7061 in
Wet to bisque shrinkage
6.4%
Bisque to final shrinkage
4.2%
Total linear shrinkage
10.33%
Isotropic volume loss
27.9%
  • Shrinkage varies with clay, forming method and firing schedule. Use a test bar fired alongside the work for a close fit.

Work through this example

Enter each loss relative to the size at the start of that stage. The two example rates combine to about 10.33% linear shrinkage.

Wet dimension = target fired dimension ÷ [(1 − wet-to-bisque loss) × (1 − bisque-to-final loss)]

Each shrinkage percentage is measured relative to the beginning of its stage. Multiply the two retained fractions to move forward, or divide by the product to work backward. Volume retention is the cube of linear retention when shrinkage is uniform in all directions.

Open the main ceramic clay calculator

Common questions

How do I extract the bisque-to-final shrinkage from two test bar readings?

Subtract the final mark spacing from the bisque mark spacing. Divide by the bisque mark spacing and multiply by 100.

Why keep the same mark spacing positions across kiln tests?

Using the same gauge features makes the before-and-after measurements comparable. Record the clay batch, forming method and firing conditions as well.