Asphalt Overlay Thickness & RAP

Compute effective pavement SN after milling, required asphalt overlay thickness, reclaimed mix supply and potential virgin binder savings.

Design readout

Effective SN
3.368
Overlay lift
3.71
in
Milled RAP
1,572.5
US tons
Binder saved
36.91
US tons

Cold-mill and overlay depth section

Cold-mill and overlay depth sectionREHABILITATION SECTIONPOST-MILL DATUMEXISTINGREHABILITATEDMILL CUT2 inRETAINED HMA5 inNEW HMA LIFT3.71 in
The mill cut removes existing HMA credit. Required overlay depth is measured from the milled surface.

RAP target supplied on site

Marker compares recovered RAP mass with target RAP demand.

Calculation ledger
Structural number to add
1.632
Pre-mill effective SN
3.94
Retained HMA thickness
5 in
New compacted overlay HMA
2,952.7 US tons
RAP to meet target blend
738.2 US tons
RAP stock surplus / shortfall
834.3 US tons
On-site RAP in new mix
25%
Virgin binder with on-site stock only
122.54 US tons
Binder savings with full target RAP
36.91 US tons

Inputs

Changes update results

Structure and mill depth
in
yd²
Existing asphalt
in
%
Existing granular support
in
%
in
%
New blend mass balance
%
%
%
%

Condition percentages multiply the intact layer coefficients. Set them using field condition and agency guidance.

How the calculation works

  1. Deduct the milled depth from existing HMA and credit the retained layers.
  2. Convert any structural number deficit to a net overlay thickness.
  3. Compare RAP supply and blend demand, then credit available RAP binder against virgin binder.

The analytical lift is a structural minimum. Confirm practical lift thickness, mix design, binder blending and stockpile processing losses with project data.

Read the equations and sources