Long-span ionoplast vision lite

A stiff ionoplast interlayer joins unequal plies over a long clear span.

Wölfel–Bennison · EN 16612 context

Inputs

Glass and support
mm
mm
mm
m
Interlayer shear modulus

Ionoplast includes products such as SentryGlas®.

Screening result

Interlayer shear measurably increases the modeled bending stiffness.

Pass
Shear transfer
98%
Defl. eff. t
24.12mm
Ply 1 stress t
24.09mm
Ply 2 stress t
24.27mm
Laminated glass section and shear couplingLaminated glass stiffness. Shear transfer 98 %. Defl. eff. t 24.12 mm. Ply 1 stress t 24.09 mm. Ply 2 stress t 24.27 mm.Two glass plies and interlayerSpan 2.85 mPly 1 · interlayer · ply 2Equivalent thicknessDeflection comparison at the same spanUncoupledEffectiveFull shearEffective t 24.12 mmInterlayer shear transferUncoupled50%Fully coupled

Calculation details

Applied interlayer shear modulus
50 MPa
Uncoupled effective thickness
13.973 mm
Fully coupled effective thickness
24.256 mm
Stiffness over uncoupled plies
5.146
Fraction of fully coupled stiffness
98.4 %

Formula trace in SI

  1. Interlayer coupling

    ω = G / (G + 9.6 E A* hv / L²)

    G = 50 MPa, reduced area per width A* = 5.455 mm, ω = 97.98 %.

  2. Equivalent bending thickness

    heff,w³ = h₁³ + h₂³ + 12ωA*H²

    Ply centroid distance H = 13.28 mm, heff,w = 24.124 mm.

  3. Surface bending stress thickness

    heff,σ,i = √[heff,w³/(hi + 2ωdi)]

    Ply 1 24.088 mm, ply 2 24.272 mm.

  4. Stiffness gain

    Ieff / Ilayered = heff,w³ / (h₁³ + h₂³)

    5.146× the uncoupled limit.