Short-span thick ionoplast laminate

A thick interlayer and short span increase the sensitivity to interlayer shear.

Wölfel–Bennison · EN 16612 context

Inputs

Glass and support
mm
mm
mm
m
Interlayer shear modulus

Ionoplast includes products such as SentryGlas®.

Screening result

Interlayer shear measurably increases the modeled bending stiffness.

Pass
Shear transfer
42.5%
Defl. eff. t
18.51mm
Ply 1 stress t
20.19mm
Ply 2 stress t
20.19mm
Laminated glass section and shear couplingLaminated glass stiffness. Shear transfer 42.5 %. Defl. eff. t 18.51 mm. Ply 1 stress t 20.19 mm. Ply 2 stress t 20.19 mm.Two glass plies and interlayerSpan 0.55 mPly 1 · interlayer · ply 2Equivalent thicknessDeflection comparison at the same spanUncoupledEffectiveFull shearEffective t 18.51 mmInterlayer shear transferUncoupled50%Fully coupled

Calculation details

Applied interlayer shear modulus
25 MPa
Uncoupled effective thickness
12.599 mm
Fully coupled effective thickness
23.022 mm
Stiffness over uncoupled plies
3.17
Fraction of fully coupled stiffness
52 %

Formula trace in SI

  1. Interlayer coupling

    ω = G / (G + 9.6 E A* hv / L²)

    G = 25 MPa, reduced area per width A* = 5 mm, ω = 42.54 %.

  2. Equivalent bending thickness

    heff,w³ = h₁³ + h₂³ + 12ωA*H²

    Ply centroid distance H = 13.04 mm, heff,w = 18.508 mm.

  3. Surface bending stress thickness

    heff,σ,i = √[heff,w³/(hi + 2ωdi)]

    Ply 1 20.194 mm, ply 2 20.194 mm.

  4. Stiffness gain

    Ieff / Ilayered = heff,w³ / (h₁³ + h₂³)

    3.17× the uncoupled limit.