ABS faceplate with equal shrinkage

An ABS faceplate uses 0.5% shrinkage in both measured directions.

Edit inputs ↓

Inputs

mm
mm
%
%
pp
Percentage points added to and subtracted from each nominal shrinkage.
mm
mm
Review calculations ↑
Steel flow
114.5729mm
Steel cross
68.3417mm
Worst error
0.1001mm
Shrink delta
0pp

Steel and molded-part dimension overlay

Live schematic
STEEL ENVELOPEMOLDED OUTLINEFlow 114.573 mmCross 68.342 mm

Within part tolerance

0%100% tolerance125%+

Compares the largest absolute error from the two worst-case bands. Directional shrink difference indicates warpage tendency.

Calculation details
Selected conventionMold basis · Lₚ ÷ (1 − S)
Flow molded minimum113.8999 mm
Flow molded maximum114.1001 mm
Cross molded minimum67.9323 mm
Cross molded maximum68.0678 mm
Part tolerance remaining0.0199 mm
Directional shrinkNo difference entered

Working through the example

Calculate steel by dividing each part target by 0.995. The longer flow dimension has a wider absolute band.

Mold basis S = (L_cav−L_part)/L_cav. Part basis S = (L_cav−L_part)/L_part. Use the same basis for the steel calculation and its inverse.

Apply the shrinkage spread in percentage points and the steel tolerance as an absolute ± dimension. The low end uses the smallest steel and greatest shrink. The high end uses the largest steel and least shrink. Compare the greatest deviation from either nominal dimension with the part tolerance. Resin presets illustrate directional inputs. Confirm values for the actual grade, flow direction, processing and conditioning.

Methodology and sources