Hot-runner PP closure shot

Sixteen closures run on a smaller screw with no cold feed mass in the shot.

Edit inputs ↓

Inputs

g
g
g/cm³
g/cm³
Use melt density at your processing condition.
mm
mm
mm
Review calculations ↑
Shot weight
70.4g
Melt volume
95.14cm³
Dose stroke
104.78mm
Barrel use
67.6%

Screw stroke and melt cushion

Live schematic
SCREW Ø 34 mmMAX 155 mmDose 104.78 mmCushion 4 mm

Within 20–80% window

<20%20–80%>80%

Below 20% raises residence-time risk. Above 80% can restrict consistent plasticizing. The cushion also has to fit.

Calculation details
Rated swept volume140.73 cm³
Equivalent solid volume77.79 cm³
Cushion volume3.63 cm³
Dose plus cushion108.78 mm
Stroke remaining46.22 mm
Melt density0.74 g/cm³

Working through the example

The melt volume is larger than the room-temperature solid volume. Millimeters of stroke follow the melt volume.

m_shot = N × m_part + m_runner. V_melt = m_shot/ρ_melt. S_dose = 1000V_melt/(πD²/4) with cm³ and mm.

The barrel rating is geometric swept volume. Utilization counts the dose only, with 20–80% inclusive. Add the target cushion separately for the travel check. The solid-density result gives an equivalent room-temperature volume. Material and machine limits can narrow the screening window.

Methodology and sources