AWS D1.1 · AISC 360
E80 eligible transverse fillet under ASD
A straight E80 weld is loaded transverse to the seam and the engineer has confirmed direction-factor eligibility.
Engineering screening only. Verify the applicable code, material and qualified WPS/PQR before production use.
Inputs
Live weld sheet
Updated from inputsLeg & weld load · 5 mm to 11 mm · 63.3 % load utilization.
Result details
| Effective throat | 4.949 mm |
|---|---|
| LRFD resistance | 331.67 kN |
| ASD allowable load | 221.11 kN |
| Applied direction factor | 1.5 |
| Nominal 0.707 × leg | 4.949 mm |
| Effective weld length | 180 mm |
| Effective throat area | 890.82 mm² |
| Electrode classification strength | 551.6 MPa |
| Angle-only factor | 1.5 |
| Nominal weld-metal resistance | 442.22 kN |
| Governing plate thickness | 13 mm |
| Minimum nominal leg | 5 mm |
| Maximum edge leg | 11 mm |
| Demand / applicable resistance | 63.3 % |
| Weld-metal load margin | 81.11 kN |
Worked example
Starting inputs
- Equal leg size
- 7 mm
- Weld length
- 180 mm
- Electrode strength
- E80xx
- Angle to weld axis
- 90 °
- Directional increase
- Eligible load path
- Demand basis
- ASD service
- Weld load demand
- 140 kN
Baseline results
- Effective throat
- 4.949 mm
- LRFD resistance
- 331.67 kN
- ASD allowable load
- 221.11 kN
- Applied direction factor
- 1.5
The 4.949 mm effective throat over 180 mm gives 890.82 mm² of weld area. With direction factor 1.5, compare the 81.11 kN signed resistance margin with zero.
Try it. At 90° the factor reaches 1.50. Use the ASD resistance with the entered service-level demand.
Calculation method
tₑ = 0.707w · LRFD = 0.75(0.60FEXX)tₑLₑk · ASD = 0.30FEXX·tₑLₑk
The angle θ is measured from the weld axis. The angle-only factor is 1 + 0.50·sin¹·⁵θ. Use 1.00 unless the selected weld condition permits the increase. Check strain compatibility for the actual weld group. AISC limits effective leg to L/4 for a short weld. For end loading, β reduces length above L/w = 100 and effective length is limited to 180w beyond L/w = 300.
The AWS screen uses the thinner piece for low-hydrogen welding and the thicker piece for the non-low-hydrogen case without qualified crack-prevention preheat. The latter case carries a single-pass condition. AISC uses the thinner piece. AWS cyclic service adds its separate minimum. The conservative edge maximum reserves 2 mm or 1/16 in at and above the corresponding quarter-inch class threshold.
The table basis fixes the inch or metric series even when you switch display units. The capacity is for one straight weld and weld metal only. Check base-metal limit states, eccentricity, fatigue and any qualified joint exceptions separately.