ASPHALTPAVELAB / PAVEMENT DESIGN WORKSHEET
Light tack on fresh asphalt
Asphalt Tonnage, Tack & Haul · US customary units
Production and tack screen met. Marker shows plant output relative to paver demand. The tack check uses the selected surface band.
Inputs
| Section length | 1,480 ft |
|---|---|
| Paving width | 11 ft |
| Compacted thickness | 1.25 in |
| Compacted mix SG Gₘᵦ | 2.42 |
| Purchase allowance | 2% |
| Receiving surface | New asphalt |
| Residual tack rate | 0.03 gal/yd² |
| Binder in supplied emulsion | 65% |
| Added water in final spray | 25% |
| Plant production | 280 US tons/h |
| Paver travel speed | 24 ft/min |
| Truck payload | 22 US tons |
| Round-trip cycle | 75 min |
Results
| Gross HMA order | 130.6 US tons |
|---|---|
| Diluted tack volume | 111.3 US gal |
| Theoretical paver rate | 124.6 US tons/h |
| Fleet at requested paver rate | 8 |
| Net compacted HMA | 128 US tons |
| Compacted mix density | 151.01 lb/ft³ |
| Tack coverage area | 1,808.9 yd² |
| Route length | 0.28 mi |
| Residual binder volume | 54.3 US gal |
| Undiluted emulsion volume | 83.5 US gal |
| Diluted distributor bar rate | 0.062 gal/yd² |
| Plant/paver limited throughput | 124.6 US tons/h |
| Fleet at feasible throughput | 8 |
| Gross mix supply time | 1.05 h |
| Reference residual tack minimum | 0.02 gal/yd² |
| Reference residual tack maximum | 0.05 gal/yd² |
Check tack rate and dilution against the contract and emulsion supplier. The steady-state haul model assumes uniform payload and cycle time.