304L composition screening
A 304L fastener lot has typical 18.2% chromium and 0.05% nitrogen. The wetted areas of the two coupled surfaces are similar.
Inputs
SI unitsEnter mass percent from the material certificate and the wetted areas exposed to the same electrolyte. Presets are typical chemistry.
- PREN
- 19
- PREN with W
- 19
- Area factor
- 1 ×
- Rate proxy
- 0.12 mm/yr
Pitting resistance and exposed areas
SchematicArea ratio is a sensitivity screen. Check the galvanic series, electrolyte, temperature, crevices and actual alloy condition.
Calculation details
- Standard PREN tier
- Below 25 · higher susceptibility
- Tungsten-adjusted tier
- Below 25 · higher susceptibility
- Galvanic area screen
- Low area contrast
- Area-scaled anode rate
- 0.12 mm/yr
Inputs used
- Alloy composition preset
- 304L stainless
- Chromium · Cr
- 18.2 %
- Molybdenum · Mo
- 0 %
- Tungsten · W
- 0 %
- Nitrogen · N
- 0.05 %
- Cathode / anode area
- 1 ×
- Uncoupled anode rate
- 0.12 mm/yr
Worked calculation
Starting values · SI- Cr + 3.3Mo + 16N = 19. The tungsten-adjusted number is 19.
- The standard PREN tier is below 25 · higher susceptibility.
- Apply the 1× area factor to 0.12 mm/yr for a rate proxy of 0.12 mm/yr.
Check the lower composition score against the actual chloride exposure. Similar wetted areas limit only the area effect.
Method and limits
Calculate each composition index
Standard PREN = Cr + 3.3Mo + 16N. With tungsten use PREN_W = Cr + 3.3(Mo + 0.5W) + 16N. Enter each element in mass percent.
Read the comparison bands
The bands are below 25, 25 to below 32, 32 to 40 inclusive, and above 40. The highest band denotes a seawater candidate for further assessment.
Compare the exposed areas
The proxy multiplies the uncoupled anode rate by max(1, cathode/anode area). Area contrast is low up to 1, raised above 1 through 10, and high above 10. These are comparison bands for the area effect.