Asymmetric acoustic PVB laminate

Different ply thicknesses shift sound coincidence and require separate bending-stress thicknesses.

Wölfel–Bennison · EN 16612 context

Inputs

Glass and support
mm
mm
mm
m
Interlayer shear modulus

Ionoplast includes products such as SentryGlas®.

MPa

0 represents the uncoupled layered limit.

Screening result

Interlayer shear measurably increases the modeled bending stiffness.

Pass
Shear transfer
31.7%
Defl. eff. t
11.67mm
Ply 1 stress t
13.96mm
Ply 2 stress t
12.16mm
Laminated glass section and shear couplingLaminated glass stiffness. Shear transfer 31.7 %. Defl. eff. t 11.67 mm. Ply 1 stress t 13.96 mm. Ply 2 stress t 12.16 mm.Two glass plies and interlayerSpan 1.65 mPly 1 · interlayer · ply 2Equivalent thicknessDeflection comparison at the same spanUncoupledEffectiveFull shearEffective t 11.67 mmInterlayer shear transferUncoupled50%Fully coupled

Calculation details

Applied interlayer shear modulus
0.28 MPa
Uncoupled effective thickness
9.488 mm
Fully coupled effective thickness
14.7 mm
Stiffness over uncoupled plies
1.862
Fraction of fully coupled stiffness
50.1 %

Formula trace in SI

  1. Interlayer coupling

    ω = G / (G + 9.6 E A* hv / L²)

    G = 0.28 MPa, reduced area per width A* = 3.214 mm, ω = 31.71 %.

  2. Equivalent bending thickness

    heff,w³ = h₁³ + h₂³ + 12ωA*H²

    Ply centroid distance H = 7.76 mm, heff,w = 11.673 mm.

  3. Surface bending stress thickness

    heff,σ,i = √[heff,w³/(hi + 2ωdi)]

    Ply 1 13.958 mm, ply 2 12.159 mm.

  4. Stiffness gain

    Ieff / Ilayered = heff,w³ / (h₁³ + h₂³)

    1.862× the uncoupled limit.