Deep glue line at a glazed lintel

A wide joint cavity is proposed to allow installation movement.

ASTM C1401 · 1:1 to 3:1

Inputs

Lite and wind suction
m
m
kPa
kPa

138 kPa is approximately 20 psi.

Movement and proposed joint
K
µm/(m·K)
%

Use the approved structural shear strain.

mm
mm

Screening result

Proposed bite must be between one and three times the glue-line thickness.

Fail
Required bite
6mm
Min. glue line
7.82mm
Bite : glue
0.75 : 1
Movement
0.98mm
Structural silicone section and joint geometryStructural silicone joint. Required bite 6 mm. Min. glue line 7.82 mm. Bite : glue 0.75 : 1. Movement 0.98 mm.Structural glazing sectionLite width 1.05 m · 1.3 kPa suctionGlassSiliconeMullionProposed bond geometryThermal travel 0.98 mmBite 9 mmGlue line 12 mmBite-to-glue ratio (1:1–3:1)0:12:14:1+

Calculation details

Wind-only structural bite
4.946 mm
Movement-only glue line
7.82 mm
Compatible bite before rounding up
7.82 mm
Compatible glue line before rounding up
7.82 mm
Governing dimensional utilization
66.7 %

Formula trace in SI

  1. Wind suction bite

    Bwind = aₛ q / (2 σallow)

    1.05 m × 1.3 kPa / (2 × 138 kPa) → 4.946 mm.

  2. Differential movement

    Δ = |αAl − αglass| × Llong/2 × ΔT

    Glass CTE 9 µm/(m·K), relative travel 0.978 mm.

  3. Glue line and limits

    Gmove = Δ/γallow; B,G ≥ 6 mm; G ≤ B ≤ 3G

    At 12.5 % shear strain, Gmove = 7.82 mm. Minimum compatible B × G = 7.82 × 7.82 mm.