Laminated glass effective-thickness calculator

Explore how interlayer shear couples two glass plies under one-way bending.

Wölfel–Bennison · EN 16612 context

Inputs

Glass and support
mm
mm
mm
m
Interlayer shear modulus

Ionoplast includes products such as SentryGlas®.

Screening result

Interlayer shear measurably increases the modeled bending stiffness.

Pass
Shear transfer
81.8%
Defl. eff. t
14.69mm
Ply 1 stress t
15.07mm
Ply 2 stress t
15.06mm
Laminated glass section and shear couplingLaminated glass stiffness. Shear transfer 81.8 %. Defl. eff. t 14.69 mm. Ply 1 stress t 15.07 mm. Ply 2 stress t 15.06 mm.Two glass plies and interlayerSpan 1.5 mPly 1 · interlayer · ply 2Equivalent thicknessDeflection comparison at the same spanUncoupledEffectiveFull shearEffective t 14.69 mmInterlayer shear transferUncoupled50%Fully coupled

Calculation details

Applied interlayer shear modulus
7 MPa
Uncoupled effective thickness
8.996 mm
Fully coupled effective thickness
15.487 mm
Stiffness over uncoupled plies
4.356
Fraction of fully coupled stiffness
85.4 %

Formula trace in SI

  1. Interlayer coupling

    ω = G / (G + 9.6 E A* hv / L²)

    G = 7 MPa, reduced area per width A* = 3.429 mm, ω = 81.81 %.

  2. Equivalent bending thickness

    heff,w³ = h₁³ + h₂³ + 12ωA*H²

    Ply centroid distance H = 8.52 mm, heff,w = 14.692 mm.

  3. Surface bending stress thickness

    heff,σ,i = √[heff,w³/(hi + 2ωdi)]

    Ply 1 15.069 mm, ply 2 15.064 mm.

  4. Stiffness gain

    Ieff / Ilayered = heff,w³ / (h₁³ + h₂³)

    4.356× the uncoupled limit.