ASME V Article 8 · ET model

Brass at the surface reference

A 50 kHz model for brass is evaluated exactly at the surface to establish a reference phase.

Reading the result. At depth zero the phase lag is zero and the current fraction is one. A depth-derived target frequency needs a nonzero depth.

Setup

Material

Use 1 for a nonmagnetic material.

Test conditions

kHz
mm
×
Use 1 for standard or 3 for effective depth.
Worked examples

Results update as you edit. Use calibrated measurements.

Inspection readout

SI units
Skin depth δ
0.55852mm
3δ depth
1.6756mm
J / J₀
100%
Phase lag
0°
Within 3δ model depth

Skin depth describes current density decay in a homogeneous half-space.

Current decay and impedance phaseThe left plot follows J/J₀ with depth. The right plot wraps phase by 360° and uses the same relative current magnitude.Induction profileδ 0.55852 mmTarget depth / δ0×EC decay3δ depthTarget phase
The left plot follows J/J₀ with depth. The right plot wraps phase by 360° and uses the same relative current magnitude.
Depth / skin depth
0×
Unwrapped phase lag
0rad
Conductivity used
16.24MS/m
Relative conductivity used
28% IACS
Frequency for target d/δ
—
  • A finite target frequency requires a nonzero target depth.

Conductivity presets are nominal at room temperature. Real coil response also depends on lift-off, geometry, frequency response and local permeability. Equations and references