ASME V Article 8 · ET model
Annealed copper conductivity standard
A room-temperature annealed copper standard is checked at 60 kHz and a 0.27 mm target.
Reading the result. The target is about one skin depth. The current fraction is close to e⁻¹.
Setup
Material
% IACS
Use 1 for a nonmagnetic material.
Test conditions
kHz
mm
×
Use 1 for standard or 3 for effective depth.
Results update as you edit. Use calibrated measurements.
Inspection readout
SI units- Skin depth δ
- 0.26979mm
- 3δ depth
- 0.80938mm
- J / J₀
- 36.76%
- Phase lag
- 57.34°
Within 3δ model depth
Skin depth describes current density decay in a homogeneous half-space.
- Depth / skin depth
- 1.0008×
- Unwrapped phase lag
- 1.0008rad
- Conductivity used
- 58MS/m
- Relative conductivity used
- 100% IACS
- Frequency for target d/δ
- 59.908kHz
Conductivity presets are nominal at room temperature. Real coil response also depends on lift-off, geometry, frequency response and local permeability. Equations and references