AWS D1.1 · AISC 360
AWS cyclic fillet minimum on a light edge
The assembly has a nominal 1/8 in fillet and is designated cyclic under the AWS detail.
Engineering screening only. Verify the applicable code, material and qualified WPS/PQR before production use.
Inputs
Live weld sheet
Updated from inputsLeg & weld load · 0.188 in to 0.2 in · 35.3 % load utilization.
Result details
| Effective throat | 0.088 in |
|---|---|
| LRFD resistance | 9.54 kip |
| ASD allowable load | 6.36 kip |
| Applied direction factor | 1 |
| Nominal 0.707 × leg | 0.088 in |
| Effective weld length | 4 in |
| Effective throat area | 0.35 in² |
| Electrode classification strength | 60 ksi |
| Angle-only factor | 1.177 |
| Nominal weld-metal resistance | 12.73 kip |
| Governing plate thickness | 0.2 in |
| Minimum nominal leg | 0.188 in |
| Maximum edge leg | 0.2 in |
| Demand / applicable resistance | 35.3 % |
| Weld-metal load margin | 6.17 kip |
Worked example
Starting inputs
- Equal leg size
- 0.125 in
- Weld length
- 4 in
- Electrode strength
- E60xx
- Angle to weld axis
- 30 °
- Weld load demand
- 3.372134 kip
- Welded edge plate
- 0.2 in
- Opposite plate
- 0.25 in
Baseline results
- Effective throat
- 0.088 in
- LRFD resistance
- 9.54 kip
- ASD allowable load
- 6.36 kip
- Applied direction factor
- 1
The 0.088 in effective throat over 4 in gives 0.35 in² of weld area. With direction factor 1, compare the 6.17 kip signed resistance margin with zero.
Try it. Changing static service to cyclic raises the minimum nominal AWS leg for this thickness band.
Calculation method
tₑ = 0.707w · LRFD = 0.75(0.60FEXX)tₑLₑk · ASD = 0.30FEXX·tₑLₑk
The angle θ is measured from the weld axis. The angle-only factor is 1 + 0.50·sin¹·⁵θ. Use 1.00 unless the selected weld condition permits the increase. Check strain compatibility for the actual weld group. AISC limits effective leg to L/4 for a short weld. For end loading, β reduces length above L/w = 100 and effective length is limited to 180w beyond L/w = 300.
The AWS screen uses the thinner piece for low-hydrogen welding and the thicker piece for the non-low-hydrogen case without qualified crack-prevention preheat. The latter case carries a single-pass condition. AISC uses the thinner piece. AWS cyclic service adds its separate minimum. The conservative edge maximum reserves 2 mm or 1/16 in at and above the corresponding quarter-inch class threshold.
The table basis fixes the inch or metric series even when you switch display units. The capacity is for one straight weld and weld metal only. Check base-metal limit states, eccentricity, fatigue and any qualified joint exceptions separately.