12.5 mm mix with excessive fines

Explore how a higher No. 200 passing percentage affects the dust-to-binder screen.

Design readout

Air voids
4
%
VMA
13.98
%
VFA
71.39
%
Eff. binder
4.27
%

Compacted mix phase blocks

Compacted mix phase blocksVOLUME FRACTIONSNMAS ½ inAIR4%EFF. BINDER10%BULK AGGREGATE86%VMA13.98%VFA71.39%DUST RATIO1.699
VMA contains air plus effective binder. Absorbed binder lies within the bulk aggregate volume.

Review VMA, dust ratio

VMA is 13.982%. Screening limit is 14% minimum.

Calculation ledger
Aggregate by mix mass
94.6%
Effective aggregate SG
2.7343
Absorbed binder by aggregate mass
1.198%
Dust-to-binder ratio
1.699
Minimum design VMA
14%
Lower design VFA limit
65%
Upper design VFA limit
78%

Inputs

Changes update results

Binder and aggregate
%
%
Measured mix and design class

Work through this example

  1. Use Rice SG and binder fractions to calculate effective aggregate SG.
  2. Compute air and mineral void volumes from the compacted specimen.
  3. Correct binder for aggregate absorption and compare the volumetric screen.

Reduce the percent passing. VMA and VFA stay fixed while the dust ratio changes.

The screen uses the FHWA Superpave workbook limits and a ±0.1 percentage-point display band about 4.0% design air voids. Verify current agency mix specifications, gyrations, moisture susceptibility and any gradation exceptions.

Read the equations and sources