316L next to a small active fastener
A 316L surface presents 16 times the wetted area of an electrically connected active fastener.
Inputs
SI unitsEnter mass percent from the material certificate and the wetted areas exposed to the same electrolyte. Presets are typical chemistry.
- PREN
- 24.93
- PREN with W
- 24.93
- Area factor
- 16 ×
- Rate proxy
- 1.92 mm/yr
Pitting resistance and exposed areas
SchematicArea ratio is a sensitivity screen. Check the galvanic series, electrolyte, temperature, crevices and actual alloy condition.
Calculation details
- Standard PREN tier
- Below 25 · higher susceptibility
- Tungsten-adjusted tier
- Below 25 · higher susceptibility
- Galvanic area screen
- High area contrast
- Area-scaled anode rate
- 1.92 mm/yr
Inputs used
- Alloy composition preset
- 316L stainless
- Chromium · Cr
- 17.2 %
- Molybdenum · Mo
- 2.1 %
- Tungsten · W
- 0 %
- Nitrogen · N
- 0.05 %
- Cathode / anode area
- 16 ×
- Uncoupled anode rate
- 0.12 mm/yr
Worked calculation
Starting values · SI- Cr + 3.3Mo + 16N = 24.93. The tungsten-adjusted number is 24.93.
- The standard PREN tier is below 25 · higher susceptibility.
- Apply the 16× area factor to 0.12 mm/yr for a rate proxy of 1.92 mm/yr.
A large noble surface can concentrate galvanic current on the active fastener. Verify the coupling in the real electrolyte.
Method and limits
Calculate each composition index
Standard PREN = Cr + 3.3Mo + 16N. With tungsten use PREN_W = Cr + 3.3(Mo + 0.5W) + 16N. Enter each element in mass percent.
Read the comparison bands
The bands are below 25, 25 to below 32, 32 to 40 inclusive, and above 40. The highest band denotes a seawater candidate for further assessment.
Compare the exposed areas
The proxy multiplies the uncoupled anode rate by max(1, cathode/anode area). Area contrast is low up to 1, raised above 1 through 10, and high above 10. These are comparison bands for the area effect.