Alloy 625 galvanic pairing

A nickel alloy connector with 21.5% Cr and 9% Mo is coupled to an exposed active steel part.

Inputs

SI units

Enter mass percent from the material certificate and the wetted areas exposed to the same electrolyte. Presets are typical chemistry.

%
%
%
%
×
mm/yr
PREN
51.2
PREN with W
51.2
Area factor
12 ×
Rate proxy
0.84 mm/yr

Pitting resistance and exposed areas

Schematic
Pitting resistance and exposed areas (schematic, not to scale)Chloride comparison bands<2525–<3232–40>40CathodeActive anodeSchematic wetted areasSTANDARD PREN51.2PREN WITH W51.2AREA RATIO12 ×
High area contrast

Area ratio is a sensitivity screen. Check the galvanic series, electrolyte, temperature, crevices and actual alloy condition.

Cathode to anode area · 10:1 reference

Calculation details

Standard PREN tier
Above 40 · seawater candidate
Tungsten-adjusted tier
Above 40 · seawater candidate
Galvanic area screen
High area contrast
Area-scaled anode rate
0.84 mm/yr

Worked calculation

Starting values · SI
  1. Cr + 3.3Mo + 16N = 51.2. The tungsten-adjusted number is 51.2.
  2. The standard PREN tier is above 40 · seawater candidate.
  3. Apply the 12× area factor to 0.07 mm/yr for a rate proxy of 0.84 mm/yr.

The composition formula is illustrative across alloy families. Prioritize actual electrochemical data when screening the connected steel.

Method and limits

  1. Calculate each composition index

    Standard PREN = Cr + 3.3Mo + 16N. With tungsten use PREN_W = Cr + 3.3(Mo + 0.5W) + 16N. Enter each element in mass percent.

  2. Read the comparison bands

    The bands are below 25, 25 to below 32, 32 to 40 inclusive, and above 40. The highest band denotes a seawater candidate for further assessment.

  3. Compare the exposed areas

    The proxy multiplies the uncoupled anode rate by max(1, cathode/anode area). Area contrast is low up to 1, raised above 1 through 10, and high above 10. These are comparison bands for the area effect.