2205 duplex alloy screen
A typical 2205 heat contains 22.0% Cr, 3.1% Mo and 0.17% N. The wetted cathode area is four times the anode area.
Inputs
SI unitsEnter mass percent from the material certificate and the wetted areas exposed to the same electrolyte. Presets are typical chemistry.
- PREN
- 34.95
- PREN with W
- 34.95
- Area factor
- 4 ×
- Rate proxy
- 0.48 mm/yr
Pitting resistance and exposed areas
SchematicArea ratio is a sensitivity screen. Check the galvanic series, electrolyte, temperature, crevices and actual alloy condition.
Calculation details
- Standard PREN tier
- 32 to 40 · higher resistance
- Tungsten-adjusted tier
- 32 to 40 · higher resistance
- Galvanic area screen
- Raised area contrast
- Area-scaled anode rate
- 0.48 mm/yr
Inputs used
- Alloy composition preset
- 2205 duplex
- Chromium · Cr
- 22 %
- Molybdenum · Mo
- 3.1 %
- Tungsten · W
- 0 %
- Nitrogen · N
- 0.17 %
- Cathode / anode area
- 4 ×
- Uncoupled anode rate
- 0.12 mm/yr
Worked calculation
Starting values · SI- Cr + 3.3Mo + 16N = 34.95. The tungsten-adjusted number is 34.95.
- The standard PREN tier is 32 to 40 · higher resistance.
- Apply the 4× area factor to 0.12 mm/yr for a rate proxy of 0.48 mm/yr.
Read the composition index and area-factor proxy as separate checks. Material selection also depends on service temperature and crevices.
Method and limits
Calculate each composition index
Standard PREN = Cr + 3.3Mo + 16N. With tungsten use PREN_W = Cr + 3.3(Mo + 0.5W) + 16N. Enter each element in mass percent.
Read the comparison bands
The bands are below 25, 25 to below 32, 32 to 40 inclusive, and above 40. The highest band denotes a seawater candidate for further assessment.
Compare the exposed areas
The proxy multiplies the uncoupled anode rate by max(1, cathode/anode area). Area contrast is low up to 1, raised above 1 through 10, and high above 10. These are comparison bands for the area effect.