CorrosionRateLab
Menu

PREN and Galvanic Area Ratio Calculator

Compare stainless, duplex and nickel alloy composition and see how an exposed cathode-to-anode area ratio changes a rate proxy.

Inputs

SI units

Enter mass percent from the material certificate and the wetted areas exposed to the same electrolyte. Presets are typical chemistry.

%
%
%
%
×
mm/yr
PREN
34.95
PREN with W
34.95
Area factor
4 ×
Rate proxy
0.48 mm/yr

Pitting resistance and exposed areas

Schematic
Pitting resistance and exposed areas (schematic, not to scale)Chloride comparison bands<2525–<3232–40>40CathodeActive anodeSchematic wetted areasSTANDARD PREN34.95PREN WITH W34.95AREA RATIO4 ×
Raised area contrast

Area ratio is a sensitivity screen. Check the galvanic series, electrolyte, temperature, crevices and actual alloy condition.

Cathode to anode area · 10:1 reference

Calculation details

Standard PREN tier
32 to 40 · higher resistance
Tungsten-adjusted tier
32 to 40 · higher resistance
Galvanic area screen
Raised area contrast
Area-scaled anode rate
0.48 mm/yr

Method and limits

  1. Calculate each composition index

    Standard PREN = Cr + 3.3Mo + 16N. With tungsten use PREN_W = Cr + 3.3(Mo + 0.5W) + 16N. Enter each element in mass percent.

  2. Read the comparison bands

    The bands are below 25, 25 to below 32, 32 to 40 inclusive, and above 40. The highest band denotes a seawater candidate for further assessment.

  3. Compare the exposed areas

    The proxy multiplies the uncoupled anode rate by max(1, cathode/anode area). Area contrast is low up to 1, raised above 1 through 10, and high above 10. These are comparison bands for the area effect.