West-facing tinted storefront

The tinted glass center sees direct afternoon sun while the frame shades the perimeter.

Solar absorption · Edge restraint

Inputs

Solar and edge conditions
W/m²
°C
°C
mm
W/(m²·K)
Glass edge
MPa

Enter a verified reference when available.

Screening result

Modeled tensile stress exceeds the selected edge allowance.

Fail
Center–edge ΔT
48.4K
Edge stress
26.34MPa
Edge allowance
15.3MPa
Safety factor
0.581
Shaded glass perimeter and center-to-edge temperaturesSolar thermal edge stress. Center–edge ΔT 48.4 K. Edge stress 26.34 MPa. Edge allowance 15.3 MPa. Safety factor 0.581.Sunlit center and cool perimeterAbsorptance 0.64Shaded band 52 mmCross-pane temperatureEdge 15 °C · center 63.4 °CEdgeCenterEdgeΔT 48.4 KEdge tensile demand0%100% limit200%+

Calculation details

Sunlit center temperature
63.4 °C
Shaded edge temperature
15 °C
Absorbed solar flux
576 W/m²
Frame restraint assumption
0.864
Edge stress utilization
172.1 %

Formula trace in SI

  1. Absorbed heat

    qsolar = α I; Tcenter = Tindoor + qsolar/heff

    Absorbed 576 W/m², center 63.4 °C.

  2. Edge tension

    σth = E αglass max(ΔT, 0) Kframe

    ΔT 48.4 K, Kframe 0.864, stress 26.337 MPa.

  3. Edge allowance

    σallow = σref × edge factor × treatment factor

    Factors 0.85 × 1, allowance 15.3 MPa.