Worked example · IEEE 80-2013 · Onderdonk

Copper-clad steel Annex benchmark

Adiabatic fault-current sizing of ground conductors using material constants and joint temperature limits.

IEEE 80 §11.3.1 gives an example of a 30% copper-clad steel conductor subjected to 1 kA for 1 s at 40 °C.

Candidate meets thermal area

The comparison uses the selected limit for Copper-clad steel · 30%.

Minimum cross-section
6.1129 mm²
Next standard size
10 mm²
Candidate utilization
61.129 %
Joint / material limit
1,084 °C

Inputs

Conductor and joint
°C
mm²
Fault duty
kA
s

Time–current thermal curves

Live schematic
Min. area6.113 mm²Next size10 mm²Utilization61.13 %Temp limit1,084 °CFUSING TIME / s0.07492.5486.30.33313RMS fault current / kACONDUCTOR CROSS-SECTIONSCandidateMinimum thermal area10 mm²6.113 mm²6 mm²16 mm²Required / candidate area61.13%
Logarithmic axes. The candidate curve and two standard-size references use equal material, joint and initial temperature.

Derived values & comparisons
Minimum in both systems6.1129 mm² / 12.064 kcmil
Next metric size10 mm²
Next AWG / kcmil size9 AWG
Candidate time at entered current2.6761 s
Candidate current at entered time1.6359 kA
Thermal I²t utilization37.368 %
Reference resistivity5.86 μΩ·cm
Volumetric heat capacity3.85 J/(cm³·°C)

Screening scope. Verify the tested connection limit, actual equivalent RMS current, fault duty, corrosion allowance and mechanical minimum. Use these checks together to specify the conductor.

Try this. Switch to US units and compare the minimum cross-section with the published 12.06 kcmil result.

Calculation method

IEEE Std 80-2013 §11.3.1, equations 45–46 and Tables 1–2. IEEE Eq. 45 gives mm² from kA, seconds, TCAP in J/(cm³·°C), ρᵣ in μΩ·cm, and Celsius temperatures. The result is converted to kcmil using 1 kcmil = 0.506707479 mm².

The log term is ln[(K₀ + Tₘ)/(K₀ + Tₐ)]. The candidate utilization is required area / entered area. The thermal-energy utilization is its square. Standard sizes round up from the unrounded area.

The brazed and bolted connection caps are screening settings. Aluminum EC-0 and 5005-H19 resistivity and temperature coefficients come from NBS Handbook 109, Table 1. The aluminum heat capacity and lower melting limits are engineering approximations. Zinc-coated rod constants serve as a galvanized-steel proxy.

Standards and model assumptions