ASME IX · EN 1011-1
Low heat input for a GTAW root
A small root bead uses GTAW and a relatively fast manual travel estimate. Test whether net energy falls below the entered floor.
Engineering screening only. Verify the applicable code, material and qualified WPS/PQR before production use.
Inputs
Live weld sheet
Updated from inputsNet heat window · 0.3 kJ/mm to 0.8 kJ/mm on an efficiency-adjusted basis.
Result details
| Net heat input | 0.262 kJ/mm |
|---|---|
| Electrical arc energy | 0.437 kJ/mm |
| Thermal efficiency | 60 % |
| Arc power | 1.06 kW |
| Energy used for check | 0.262 kJ/mm |
| Solid steel wire feed (mass) | — |
| Estimated net wire deposition | — |
| Entered window minimum | 0.3 kJ/mm |
| Entered window maximum | 0.8 kJ/mm |
| Distance to nearest bound | -0.038 kJ/mm |
Worked example
Starting inputs
- Welding process
- GTAW
- Arc voltage
- 12 V
- Arc current
- 88 A
- Travel speed
- 145 mm/min
- Minimum energy
- 0.3 kJ/mm
- Maximum energy
- 0.8 kJ/mm
Baseline results
- Net heat input
- 0.262 kJ/mm
- Electrical arc energy
- 0.437 kJ/mm
- Thermal efficiency
- 60 %
- Arc power
- 1.06 kW
With 1.06 kW at 145 mm/min travel, electrical arc energy is 0.437 kJ/mm. The 60 % process factor gives 0.262 kJ/mm of net heat input.
Try it. Reducing travel can raise heat input above the floor. Any production change still needs to fit the qualified procedure.
Calculation method
Arc energy = 60P / v · Net heat input = η × 60P / v
Use P in kW and travel v in mm/min for kJ/mm. Electrical power comes from V × I / 1,000 or from measured mean instantaneous V × I during the run. For waveform-controlled welding, use the acquisition method required by the governing procedure.
Planning thermal factors are SAW 1.00, GMAW/FCAW/SMAW 0.80 and GTAW 0.60. Use WPS bounds expressed on the same basis as the selected result. Wire figures use a solid-steel equivalent of 7,850 kg/m³. Tubular wire needs measured linear mass for a production estimate.