Live weld sheet
Updated from inputsCooling time window · 5 s to 25 s entered for this steel.
Result details
| Predicted t₈/₅ | 7.48 s |
|---|---|
| Governing heat flow | 2D |
| Transition thickness | 15.66 mm |
| Cold-cracking flag | Lower |
| 2D cooling estimate | 7.48 s |
| 3D cooling estimate | 5.98 s |
| Weld shape factor F₂ | 0.9 |
| Weld shape factor F₃ | 0.9 |
| Mean cooling rate | 40.11 °C/s |
| HAZ hardening tendency | Lower |
| Distance to nearest time bound | 2.48 s |
Calculation method
t₃ = (6700 − 5T₀)Q·Δ(1/T)·F₃ · t₂ = (4300 − 4.3T₀)10⁵(Q/d)²·Δ(1/T²)·F₂
Use temperature differences 500 − T₀ and 800 − T₀. Solve t₂ = t₃ for transition thickness. Below the transition, use the thin-plate 2D result. Above it, use the thick-plate 3D result. Seam factors are 1.0/1.0 for run on plate and 0.90/0.90 for butt welds. Corner and T-fillet 2D factors are midrange planning choices (0.80 and 0.55); both use 0.67 for 3D.
The qualitative hardening flag combines cooling below the entered minimum with CE(IIW) bands of 0.40 and 0.50. The cracking flag also adds hydrogen class and high restraint. Select cooling limits for the actual steel. Use grade-specific HAZ hardness, toughness and representative procedure tests for acceptance.