ASME IX · EN 1011-1
SAW longitudinal seam at high power
A mechanized submerged-arc run uses a high-current electrode on a long shop seam.
Engineering screening only. Verify the applicable code, material and qualified WPS/PQR before production use.
Inputs
Live weld sheet
Updated from inputsNet heat window · 30.48 kJ/in to 55.88 kJ/in on an efficiency-adjusted basis.
Result details
| Net heat input | 49.6 kJ/in |
|---|---|
| Electrical arc energy | 49.6 kJ/in |
| Thermal efficiency | 100 % |
| Arc power | 19.84 kW |
| Energy used for check | 49.6 kJ/in |
| Solid steel wire feed (mass) | 22.55 lb/h |
| Estimated net wire deposition | 22.1 lb/h |
| Entered window minimum | 30.48 kJ/in |
| Entered window maximum | 55.88 kJ/in |
| Distance to nearest bound | 6.28 kJ/in |
Worked example
Starting inputs
- Welding process
- SAW
- Arc voltage
- 32 V
- Arc current
- 620 A
- Travel speed
- 24 in/min
- Wire diameter
- 0.125984 in
- Wire feed speed
- 106.299213 in/min
- Minimum energy
- 30.48 kJ/in
Baseline results
- Net heat input
- 49.6 kJ/in
- Electrical arc energy
- 49.6 kJ/in
- Thermal efficiency
- 100 %
- Arc power
- 19.84 kW
With 19.84 kW at 24 in/min travel, electrical arc energy is 49.6 kJ/in. The 100 % process factor gives 49.6 kJ/in of net heat input.
Try it. With the 1.00 planning factor, arc energy and net heat input coincide numerically.
Calculation method
Arc energy = 60P / v · Net heat input = η × 60P / v
Use P in kW and travel v in mm/min for kJ/mm. Electrical power comes from V × I / 1,000 or from measured mean instantaneous V × I during the run. For waveform-controlled welding, use the acquisition method required by the governing procedure.
Planning thermal factors are SAW 1.00, GMAW/FCAW/SMAW 0.80 and GTAW 0.60. Use WPS bounds expressed on the same basis as the selected result. Wire figures use a solid-steel equivalent of 7,850 kg/m³. Tubular wire needs measured linear mass for a production estimate.