Custom material with fitted loss coefficients

Enter a custom material fit with coefficients for Hz, tesla and W/m³.

Design inputs

Winding & geometry
Excitation & material

Use W/m³ with f in Hz and B in tesla.

View live readout ↑

Live readout

Edit inputs
Peak flux
153.4 mT
Flux headroom
57.39 %
Air gap
1.586 mm
Core loss
0.07655 W
Core magnetization Core magnetization B–H reference BField H → Core gapPeak B153 mTSaturation360 mTAir gap1.59 mm
The B–H curve and gap are illustrative. The marker and labels follow the calculated flux and the selected material threshold.
Flux headroom available

Saturation uses the selected threshold. Check flux and inductance at operating temperature.

Peak flux / saturation153.4 mT / 360 mT

AC flux amplitude / saturation32.39 mT / 360 mT

Result breakdown
Peak flux density153.409 mT
Minimum flux density88.6364 mT
AC flux swing (peak-to-peak)64.7727 mT
AC flux amplitude32.3864 mT
Midpoint DC current7.1 A
DC magnetizing field2,603.33 A/m
Material saturation threshold360 mT
Peak-flux headroom206.591 mT
Peak-flux headroom57.3864 %
Relative permeability used1,650
Equivalent discrete air gap1.58554 mm
Estimated ungapped inductance1,204.26 µH
Steinmetz coefficient k2.1
Steinmetz frequency exponent α1.4
Steinmetz flux exponent β2.28
Modeled magnetic loss density17,720.4 W/m³
Modeled core loss0.0765521 W

Worked calculation

Bmax = 27 µH × 9 A / (22 × 72 mm²) = 153.409 mT

Change β while holding frequency and flux fixed to check sensitivity to the material fit.

Flux

Bmax = L·Ipk/(N·Ae) | ΔB = L·ΔIpp/(N·Ae)

Compare the absolute endpoint flux with the saturation threshold. A bipolar peak-to-peak swing can exceed that threshold while both endpoints stay within it. Hdc = N·Idc/ℓe uses the midpoint of the entered triangular current. Use it with the actual powder-core DC-bias curve and enter inductance at the operating bias.

Gap

ℓg = μ₀·N²·Ae/L − ℓe/μr

If the computed gap is negative, the ungapped core cannot reach the target L at this turn count. The estimate neglects fringing and uses linear permeability. For a powder core the result is an equivalent reluctance, not a machining dimension.

Core loss

Pcore = Ve · k · fs^α · (ΔB/2)^β

Enter frequency in Hz and flux in tesla when fitting custom coefficients for a loss density in W/m³. Ferrite coefficients are approximate fits to typical hot datasheet points. Powder presets use published coefficients for representative 60-permeability toroids. Use your exact material, geometry, temperature and waveform for final loss estimates.