High Flux choke for a 22 A peak

A high-current inductor uses a representative High Flux powder grade.

Design inputs

Winding & geometry
Excitation & material
View live readout ↑

Live readout

Edit inputs
Peak flux
203.7 mT
Flux headroom
86.42 %
Air gap
2.905 mm
Core loss
0.1336 W
Core magnetization Core magnetization B–H reference BField H → Equivalent gapPeak B204 mTSaturation1500 mTAir gap2.9 mm
The B–H curve and gap are illustrative. The marker and labels follow the calculated flux and the selected material threshold.
Flux headroom available

The gap is an equivalent reluctance. Use the powder core DC-bias curve for actual inductance.

Peak flux / saturation203.7 mT / 1,500 mT

AC flux amplitude / saturation23.15 mT / 1,500 mT

Result breakdown
Peak flux density203.704 mT
Minimum flux density157.407 mT
AC flux swing (peak-to-peak)46.2963 mT
AC flux amplitude23.1481 mT
Midpoint DC current19.5 A
DC magnetizing field8,357.14 A/m
Material saturation threshold1,500 mT
Peak-flux headroom1,296.3 mT
Peak-flux headroom86.4198 %
Relative permeability used60
Equivalent discrete air gap2.90484 mm
Estimated ungapped inductance87.2465 µH
Steinmetz coefficient k28.7665
Steinmetz frequency exponent α1.311
Steinmetz flux exponent β2.218
Modeled magnetic loss density21,203 W/m³
Modeled core loss0.133579 W

Worked calculation

Bmax = 25 µH × 22 A / (30 × 90 mm²) = 203.704 mT

Compare the saturation headroom with the AC core-loss estimate. Bias droop and winding heat still need their own checks.

Flux

Bmax = L·Ipk/(N·Ae) | ΔB = L·ΔIpp/(N·Ae)

Compare the absolute endpoint flux with the saturation threshold. A bipolar peak-to-peak swing can exceed that threshold while both endpoints stay within it. Hdc = N·Idc/ℓe uses the midpoint of the entered triangular current. Use it with the actual powder-core DC-bias curve and enter inductance at the operating bias.

Gap

ℓg = μ₀·N²·Ae/L − ℓe/μr

If the computed gap is negative, the ungapped core cannot reach the target L at this turn count. The estimate neglects fringing and uses linear permeability. For a powder core the result is an equivalent reluctance, not a machining dimension.

Core loss

Pcore = Ve · k · fs^α · (ΔB/2)^β

Enter frequency in Hz and flux in tesla when fitting custom coefficients for a loss density in W/m³. Ferrite coefficients are approximate fits to typical hot datasheet points. Powder presets use published coefficients for representative 60-permeability toroids. Use your exact material, geometry, temperature and waveform for final loss estimates.