WeldMetalLab

EN 1011-2 · Rosenthal

High interpass heat on a thin seam

A thin butt joint is evaluated for a hot interpass condition before another run.

Engineering screening only. Verify the applicable code, material and qualified WPS/PQR before production use.

Inputs

Thermal inputs
°C
kJ/mm
mm
Screening window
s
s
%

Live weld sheet

Updated from inputs
HAZ cooling curvePredicted t₈/₅ 166.56 s. Governing heat flow 2D. Transition thickness 24.55 mm. Cold-cracking flag Lower T₈/₅166.56sHEAT FLOW2DTRANSITION24.55mmCRACK FLAGLower HAZ COOLING CURVE 800650500°Ctime →Start 220 °C2D · 166.56 s2D heat flow COOLING TIME WINDOWFAIL
Outside screen

Cooling time window · 6 s to 24 s entered for this steel.

Result details

Predicted t₈/₅166.56 s
Governing heat flow2D
Transition thickness24.55 mm
Cold-cracking flagLower
2D cooling estimate166.56 s
3D cooling estimate17.69 s
Weld shape factor F₂0.9
Weld shape factor F₃0.9
Mean cooling rate1.8 °C/s
HAZ hardening tendencyLower
Distance to nearest time bound-142.56 s

Worked example

Starting inputs

Seam shape
Butt weld
Starting temperature
220 °C
Effective heat input
1.9 kJ/mm
Plate thickness
8 mm
Minimum t₈/₅
6 s
Maximum t₈/₅
24 s
CE(IIW)
0.37 %

Baseline results

Predicted t₈/₅
166.56 s
Governing heat flow
2D
Transition thickness
24.55 mm
Cold-cracking flag
Lower

At 8 mm the 2D estimate is 166.56 s and the 3D estimate is 17.69 s. The transition at 24.55 mm selects the 2D result for the screen.

Try it. The upper cooling-time bound can be exceeded even when the cracking flag is lower. The two checks address different concerns.

Calculation method

t₃ = (6700 − 5T₀)Q·Δ(1/T)·F₃ · t₂ = (4300 − 4.3T₀)10⁵(Q/d)²·Δ(1/T²)·F₂

Use temperature differences 500 − T₀ and 800 − T₀. Solve t₂ = t₃ for transition thickness. Below the transition, use the thin-plate 2D result. Above it, use the thick-plate 3D result. Seam factors are 1.0/1.0 for run on plate and 0.90/0.90 for butt welds. Corner and T-fillet 2D factors are midrange planning choices (0.80 and 0.55); both use 0.67 for 3D.

The qualitative hardening flag combines cooling below the entered minimum with CE(IIW) bands of 0.40 and 0.50. The cracking flag also adds hydrogen class and high restraint. Select cooling limits for the actual steel. Use grade-specific HAZ hardness, toughness and representative procedure tests for acceptance.

References

More worked examples