PC40 ferrite close to its hot flux limit

Assess PC40 ferrite at high DC bias using the representative hot saturation threshold.

Design inputs

Winding & geometry
Excitation & material
View live readout ↑

Live readout

Edit inputs
Peak flux
350.2 mT
Flux headroom
7.841 %
Air gap
0.7611 mm
Core loss
0.06335 W
Core magnetization Core magnetization B–H reference BField H → Core gapPeak B350 mTSaturation380 mTAir gap0.761 mm
The B–H curve and gap are illustrative. The marker and labels follow the calculated flux and the selected material threshold.
Low flux headroom

Saturation uses the selected threshold. Check flux and inductance at operating temperature.

Peak flux / saturation350.2 mT / 380 mT

AC flux amplitude / saturation35.92 mT / 380 mT

Result breakdown
Peak flux density350.204 mT
Minimum flux density278.367 mT
AC flux swing (peak-to-peak)71.8367 mT
AC flux amplitude35.9184 mT
Midpoint DC current14 A
DC magnetizing field3,769.23 A/m
Material saturation threshold380 mT
Peak-flux headroom29.7959 mT
Peak-flux headroom7.84103 %
Relative permeability used2,300
Equivalent discrete air gap0.761076 mm
Estimated ungapped inductance762.585 µH
Steinmetz coefficient k4.11814
Steinmetz frequency exponent α1.29248
Steinmetz flux exponent β2.08
Modeled magnetic loss density17,402.8 W/m³
Modeled core loss0.0633462 W

Worked calculation

Bmax = 22 µH × 15.6 A / (14 × 70 mm²) = 350.204 mT

The headroom bar is near its limit. Compare more turns at fixed inductance and note the changed gap.

Flux

Bmax = L·Ipk/(N·Ae) | ΔB = L·ΔIpp/(N·Ae)

Compare the absolute endpoint flux with the saturation threshold. A bipolar peak-to-peak swing can exceed that threshold while both endpoints stay within it. Hdc = N·Idc/ℓe uses the midpoint of the entered triangular current. Use it with the actual powder-core DC-bias curve and enter inductance at the operating bias.

Gap

ℓg = μ₀·N²·Ae/L − ℓe/μr

If the computed gap is negative, the ungapped core cannot reach the target L at this turn count. The estimate neglects fringing and uses linear permeability. For a powder core the result is an equivalent reluctance, not a machining dimension.

Core loss

Pcore = Ve · k · fs^α · (ΔB/2)^β

Enter frequency in Hz and flux in tesla when fitting custom coefficients for a loss density in W/m³. Ferrite coefficients are approximate fits to typical hot datasheet points. Powder presets use published coefficients for representative 60-permeability toroids. Use your exact material, geometry, temperature and waveform for final loss estimates.